Lambda holds a series of both U.S. and foreign patents pertaining to burnishing and surface enhancement techniques and has additional patents pending in both the U.S. and abroad.

 

U.S. patents issued to Lambda Technologies

 

Date of Patent
Patent Number
Patent Title
October 17, 2017 No. 9,789,582 Method and Compression Apparatus for Introducing Residual Compression into a Component Having a Regular or an Irregular Shaped Surface
March 15, 2016 No. 9,283,650 Burnishing Tool and Method for Burnishing
December 10, 2013 No. 8,601,659 Burnishing Tool and Method for Burnishing
August 20, 2013 No. 8,511,130 Method for Preventing and Arresting Crack Development
and Propagation
February 19, 2013 No. 8,375,805 Method and Apparatus for Sensing Distortion
November 13, 2012 No. 8,307,681 Integrally Rotating Turbo Machinery and Method and Apparatus for Achieving the Same
October 11, 2011 No. 8,033,152 Metallic Article with Improved Fatigue Performance and Corrosion Resistance
October 5, 2010 No. 7,805,972 Integrally Bladed Rotating Turbo Machinery and Method and Apparatus for Achieving the Same
July 27, 2010 No. 7,762,113 Metallic Article with Improved Fatigue Performance and Corrosion Resistance and Method for Making the Same
October 13, 2009 No. 7,600,404 Surface Treatment Apparatus and Method
June 23, 2009 No. 7,549,345 Method and Apparatus for Sensing Distortion
May 15, 2007 No. 7,219,044 Method and System for Improving a Part’s Resistance to Stress Induced Failure.
March 13, 2007 No. 7,188,398 Method for Improving the Magnitude of Compressive Stress Developed in the Surface of a Part.
January 9, 2007 No. 7,159,425 Method and Apparatus for Providing a Layer of Compressive Residual Stress in the Surface of a Part.
August 9, 2005 No. 6,926,970 Apparatus and Method for Forming Weld Joints having Compressive Residual Stress Patterns.
September 23, 2003 No. 6,622,570 Method for Reducing Tensile Stress Zones in the Surface of a Part.
July 9, 2002 No. 6,415,486 Method and Apparatus for Providing a Residual Stress Distribution in the Surface of a Part.
October 27, 1998 No. 5,826,453 Burnishing Method and Apparatus for Providing a Layer of Compressive Residual Stress in the Surface of a Workpiece.
April 7, 1998 No. 5,737,385 Automated System for Use in the Determination of Subsurface Material Properties by X-Ray Diffraction.

 

Subscribe to our Mailing List

Thank you for subscribing!

Lambda Techs
Privacy Overview

This website uses cookies so that we can provide you with the best user experience possible. Cookie information is stored in your browser and performs functions such as recognising you when you return to our website and helping our team to understand which sections of the website you find most interesting and useful.